Here is a LINK to an informative article that has to do with galvanic corrosion. This subject was brought to our attention in a comment under the Quad Tips #1 post. It seems that putting stainless steel screws into aluminum will cause the aluminum to corrode. But there are ways to get around the corrosion if you use plating or tapes.

2 comments:

NDammitt said...

I always thought that dielectric grease might do the trick too.

Simon Hawk said...

Cohort and I had talked about that as well.